So Dad bought a gallon (or so) of this 60 Grit Aluminum Oxide Blast Media for the little sandblaster and that shit worked like a charm. It took me maybe an hour to do the whole head fairing. I ran out of media but at least we know it works. So I'm getting a couple more containers to finish up the rest of the sanding with that stuff. I should have all the parts sanded and ready for primer by the end of the day. I'd drop a picture in here of the head fairing but its really just still white only more dull.
Sand blasting is definitely the way to go for hard to reach places and for all the joints, edges and holes.